Process and Service

* Iron phosphate solution (heated) always used.

* Deionized water rinse leaves parts free of surface contaminants.

* In House Sandblasting.

* Standard coating thickness range of 2 mils to 5 mils

* Powder Coated Products are cured at elevated temperatures between 3200 and 4250 degrees Fahrenheit.

* Parts are fully cured when they leave the oven.

* Local  pick-up and delivery service available.


* Our technical coating specialist can make visits to  your facility to assess your total coating needs.